SWRA705 August 2021 AWR1243 , AWR1443 , AWR1642 , AWR1843 , AWR1843AOP , AWR2243 , AWR2944 , AWR6443 , AWR6843 , AWR6843AOP , AWRL1432 , AWRL6432 , IWR1443 , IWR1642 , IWR1843 , IWR2243 , IWR6243 , IWR6443 , IWR6843 , IWR6843AOP , IWRL6432 , IWRL6432AOP
A radome with 2 mm thickness is chosen with ABS plastic material construction. Figure 6-1 shows the picture of this radome. Experiments are conducted centered around 62 GHz frequency on an IWR6843ISK EVM board.
Figure 6-2 shows two graphs with the ABS plastic rectangular radome. Figure 6-3 shows antenna radiation pattern without the radome and, correspondingly, Figure 6-2 shows antenna radiation patterns with the radome. It can be seen from the plots that this radome significantly degraded the antenna radiation pattern.